Material

KT N30UH Nd-Fe-B Magnet

Remanence Br

kGs

11.21±0.1

~1.12T

Coercivity Hcb

kOe

10.89±0.1

~866.8kA/m

Intrinsic coercivity Hcj

kOe

26.78±0.5

~2131.7 kA/m

Maximum energy product 

MGOe

31±0.5

~242.8 kJ/m3

Temp. coefficient of Br(20-150 ℃)

%/℃

-0.104


Temp. coefficient of Hcj(20-150 ℃)

%/℃

-0.470