Material | KT N40SH Nd-Fe-B | ||
Remanence Br | kGs | 12.75±0.1 | ~1.27T |
Coercivity Hcb | kOe | 12.37±0.1 | ~984.7 kA/m |
Intrinsic coercivity Hcj | kOe | 22.55±0.5 | ~1874.6 kA/m |
Maximum energy product | MGOe | 39.3±1 | ~313.2 kJ/m3 |
Temp. coefficient of Br(20-120 ℃) | %/℃ | -0.103 | |
Temp. coefficient of Hcj(20-120 ℃) | %/℃ | -0.548 |