Material

KT N38SH Nd-Fe-B



Remanence Br

kGs

12.50±0.1

~1.25T

Coercivity Hcb

kOe

12.14±0.1

~966.3 kA/m

Intrinsic coercivity Hcj

kOe

22.38±0.5

~1781.4 kA/m

Maximum energy product 

MGOe

38±0.5

~300.8 kJ/m3

Temp. coefficient of Br(20-120 ℃)

%/℃

-0.120


Temp. coefficient of Hcj(20-120 ℃)

%/℃

-0.594